Deep Black Coatings without Milling | | PCI Magazine
A paste with 13% specialty carbon black is prepared by mixing COLOUR BLACK OE 430 W with water and deer using a highspeed mixer for 10 min. There is no longer a need for intensive milling with a media mill. Milling would only result in decomposition of the preparation and ingredients, and thus would worsen performance.