Dispersion of Carbon Nanotubes Improved by Ball Milling to Prepare ...
It was then subjected to ball milling at 400 rpm for 12 h in a zirconia ballmilling container. In a glass container, epoxy/CNT mixtures were transferred to jeffamineD2000 (hardener) at a weight ratio of 19:50 (E51: D2000). ... China); the strain rate was set to mm/min, and the tension machine was equipped with two 2 KN load components ...